Diagnosis · failed 3D print
What went wrong with your 3D print? Diagnose it from a photo
Stringing, layer shift, a part that popped off the bed: upload a photo of the failed print and the AI ranks up to three likely causes, each with the setting to look for in your slicer and the values to try. The defect guide works with no account at all.
- Free defect guide, no account
- 3 photo checks a day with a free account
- 20 a day for subscribers
How it works
Pick the defect, or switch to a photo
The tool opens in filament mode. If you recognize the defect, click it in the guide to see its causes and settings, no account needed. If you don't, open the "Analyze a photo" tab.
Shoot the defect up close
Defect sharp and centered, side light so the layer lines stand out, as a JPEG, PNG or WebP. The photo is scaled down to 1024 pixels in your browser and its metadata (location, device) is stripped before upload.
Add the material and a short note
Both are optional and both help: PLA, PETG, ABS/ASA, TPU or nylon, then a note such as "PETG at 240 °C, starts about 3 cm up". The photo check needs a free account with a confirmed email address.
Try the top lead, and only that one
You get up to three causes ranked by confidence, what the AI sees in the photo and the settings to change. Change a single setting, print a small test piece, and only move to the next lead if the defect is still there.
Filament print defects: the usual cause and the first fix
| Symptom | Most common cause | First setting to try |
|---|---|---|
| Stringing | Not enough retraction | Retraction distance: +0.5 mm per test (direct drive 0.5–2 mm, Bowden 4–7 mm) |
| Warping | Dirty or greasy bed | Isopropyl alcohol on the bed before every print, and no fingers on the surface |
| Layer shift | The nozzle hits the print | Z hop of 0.2–0.4 mm, only over printed areas |
| Elephant's foot | First layer squished too much | Z offset: +0.02 to +0.05 mm per test |
| Under-extrusion | Partly clogged or worn nozzle | Cold pull at about 90 °C for PLA, or a new nozzle |
| Over-extrusion | Flow too high | Flow: −2 to −5 % per test, checked on a calibration cube |
| Z banding | Uneven Z axis | Clean, straight lead screw; layer heights in multiples of 0.04 mm |
| Ghosting / ringing | Speed or acceleration too high | Speed −20 %; acceleration of 500–1,500 mm/s² without input shaping |
| First layer not sticking | First layer too high | Z offset: −0.02 to −0.05 mm per test; first layer at 15–25 mm/s |
| Spaghetti (print came loose) | Dirty or greasy bed | Degreased bed, then a 5–10 mm brim |
| Zits and blobs | Seam and wall starts | Aligned or rear seam; extra prime after retraction set to 0 |
| Gaps in the top surface | Top skin too thin | At least 0.8–1 mm of solid top: 5 layers at 0.2 mm |
| Pillowing | Not enough cooling | Part fan at 100 % for PLA; minimum layer time of 8–10 s |
| Sagging bridges | Bridge settings off | Bridges at 25–40 mm/s, 85–95 % flow, fan at 100 % |
| Curling overhangs | Not enough cooling | Part fan: PLA 100 %, PETG 30–60 %, ABS/ASA 0–20 % |
| Failed supports | Supports too weak | 15–20 % density, 2–3 interface layers |
| Clogged nozzle | Debris in the nozzle or a worn nozzle | Repeat cold pulls until the tip comes out clean, or fit a new nozzle |
| Wet filament | Moisture soaked up by the spool | Dry it: PLA 45–50 °C, PETG 60–65 °C, ABS/ASA 70–80 °C, for 4–6 h |
Settings, hardware or material? Read the defect before you open the slicer
- It shows up at the same height across the whole part: look at the hardware (belts, pulleys, Z axis) or a nozzle strike, not at the profile.
- It follows the geometry (corners, overhangs, bridges, top surfaces): almost always speed, cooling or temperature.
- It's there from the first layer: sort out Z offset and a clean bed first, since everything above depends on them.
- The nozzle pops or crackles and the surface comes out matte, rough and bubbly: dry the spool before touching any setting.
What the AI reads in a photo, and what it can't know
The vision model never writes a setting: it picks symptom and cause pairs from the same closed list as the guide, and the tool shows the settings stored for that cause.
It only sees one image: not your G-code, not your profile, not the clicking of your extruder. A loose belt or a worn nozzle gets confirmed on the printer itself. When nothing is clear, the answer says so instead of inventing a problem, and a photo that isn't a 3D print is turned down.
A resin part is recognized: the check switches to resin causes without using up another analysis. The photo is analyzed by our AI provider (OpenAI); Nyzora keeps neither the photo nor the diagnosis.
A defect that comes from the file (holes in the mesh, a wall thinner than the nozzle) can't be fixed in the slicer: check the STL before you reprint.
What's free, what's paid
- Defect guide
- Free, no account
- Photo check
- 3 a day, free account
- Subscribers
- 20 a day
The defect guide runs in your browser, with no account. Diagnosing a photo with AI goes through our servers, then our AI provider (OpenAI): it needs a free account and has a daily limit.
A full 3D model, with AI
A well-prepared model avoids a lot of failed prints. The Nyzora studio uses AI to build a full 3D model from a photo or a sentence: 190 free credits at sign-up, with a quote before every charge.
Frequently asked questions
- Why won't my first layer stick to the bed?
- Most of the time the nozzle is too high, so the filament lands as round beads instead of being squished. Lower the Z offset by 0.02–0.05 mm per test until the lines are flat and touch each other, wipe the bed with isopropyl alcohol and print the first layer at 15–25 mm/s. Bed at 55–60 °C for PLA, 70–85 °C for PETG.
- How do I stop PETG stringing?
- PETG strings more than PLA even when it's tuned well. In this order: dry the spool (60–65 °C for 4–6 h), drop the nozzle by 5 °C while staying in the maker's range, then add 0.5 mm of retraction per test.
- My print shifted halfway up. Is it the slicer?
- Rarely. Layer shift almost always comes from the printer: the nozzle hit a curled edge (0.2–0.4 mm Z hop), an X or Y belt is loose (plucked, it should give a low, clean note), or the speed is more than the motors can handle (−20 %).
- Do the settings use my slicer's names?
- They use the common slicer vocabulary: Z offset, brim, wipe, pressure advance, retraction distance. Menus differ between programs, so type the name into the settings search of Cura, PrusaSlicer, OrcaSlicer or Bambu Studio.
- How accurate is the photo diagnosis?
- It gives likely causes with a confidence level, not certainty. Some defects look alike in a photo (under-extrusion and wet filament, ghosting and a loose belt), so test the top lead on its own before the next one. A free account gets 3 analyses a day, enough to compare two angles of the same defect.
- What's free, and what do I pay for?
- The defect guide is free, with no account. The AI photo check is free with an account: 3 a day, 20 for subscribers.
- Is my photo uploaded?
- For the AI diagnosis, yes: the photo and any details you add go through our servers, with your account, and are analyzed by our AI provider (OpenAI). Nyzora does not keep them. The defect guide needs no photo and no account.