Diagnosis · failed resin print
Resin print failed? Find the cause from a photo
Resin failures don't look like filament ones: a print left on the FEP, layers that split, suction-cup craters, a tacky surface after curing. Pick the symptom with no account, or upload a photo: the answer comes in exposure, bottom layers, lift and washing, with values to try.
- Free defect guide, no account
- 3 photo checks a day with a free account
- 20 a day for subscribers
How it works
Pin down when it failed
During the print (nothing on the plate, split layers, snapped supports) or after washing and curing (tacky surface, white haze, cracks): the causes are not the same. On this page the guide opens straight on resin defects, no account needed.
Photograph the part before cleaning it
Straight out of the vat, or still stuck to the film: broken supports, lift marks and craters are all clues. Keep nitrile gloves on until the resin is washed off.
Add the resin and your settings
Pick standard, tough (ABS-like) or water-washable resin, then add a note: exposure time, number of bottom layers, room temperature. The photo check needs a free account with a confirmed email address; the photo is analyzed by our AI provider (OpenAI), and Nyzora keeps neither the photo nor the diagnosis.
Confirm on a calibration print
Change one setting, then print a small exposure calibration part before relaunching the big one: the test costs a few milliliters of resin, while a full failure can ruin the FEP film.
The 9 resin defects: main cause and first fix
| Symptom | Most common cause | First setting to try |
|---|---|---|
| Print not on the plate, left on the FEP | Bottom layers underexposed | Bottom exposure: +5 to +10 s per test |
| Delamination | Layers underexposed | Normal exposure: +0.2 to +0.5 s per test |
| Suction cup effect | Closed hollow part | At least 2 drain holes of 3–5 mm, one near the plate and one on the far side |
| Broken supports | Supports too thin or too few | Contact tips of 0.3–0.5 mm for details, 0.5–0.8 mm for heavy parts |
| Elephant's foot (resin) | Bottom layers overexposed | Bottom exposure: −5 s per test, as long as adhesion holds |
| Cracks | Over-curing | UV kept to 2–5 min per side for a small part, turning it as you go |
| Tacky resin | Not washed enough | Two baths of 90 %+ isopropyl alcohol, the second one clean |
| White haze or cloudiness | Still wet under UV | Let it air-dry for 30–60 min before curing |
| Warped part | Supports too thin or too few | More supports under low points, and no island starting in mid-air |
Starting settings for standard resin on an MSLA printer
| Setting | Starting value | When to change it |
|---|---|---|
| Bottom exposure | 20–40 s, over 4–6 layers | Print left on the FEP: +5 to 10 s; flared base: −5 s |
| Normal exposure | The value on the resin's data sheet | Split layers or snapped supports: +0.2 to +0.5 s |
| Layer height | 0.05 mm | Cures more reliably than 0.1 mm at the same exposure |
| Lift speed | 40–60 mm/min | Slower on bottom layers and large cross-sections |
| Lift distance and rest | 6–8 mm, then a 0.5–1 s rest | Torn layers, thick or cold resin |
| Resin temperature | 22–30 °C in the vat | Room below 20 °C: warm it up, or add 10 % exposure |
| Isopropyl alcohol wash | 2 baths of 2–3 min | Never more than 10 min in total, or the surface turns white |
| UV cure at 405 nm, dry part | 2–5 min per side | Up to 10 min in total for a large part |
FEP film and vat: the check before you print again
- Tap the film: it should sound like a drum. A slack film holds on to layers instead of letting them go.
- Hold it up to a lamp: a scratch, a cloudy patch or a dent makes the same area fail on every print, and means a new film.
- Scrape the vat floor with a plastic spatula, never metal: a forgotten cured chunk gets crushed by the next layer and can puncture the film.
- After a failure, filter the resin before pouring it back, then shake the bottle for 1–2 min and stir the vat.
- If nothing stuck at all, re-level: loosen the plate, sheet of paper on the screen, home to zero, then tighten.
Delamination, suction or supports: three failures that look alike
Delamination: the part splits cleanly at one height, across its whole section; the bottom printed fine and the top stayed on the film. Check normal exposure and lift speed first.
Suction cup: a hole or crater, always in the same spot, at the bottom of a hollow shape or under a large flat area. Exposure isn't the problem: let air in through drain holes, or tilt the part 30–45°.
Broken supports: tips left on the raft, details missing or dangling. Thicker tips, more supports under low points, and a hunt for islands in the slicer.
What's free, what's paid
- Defect guide
- Free, no account
- Photo check
- 3 a day, free account
- Subscribers
- 20 a day
The defect guide runs in your browser, with no account. Diagnosing a photo with AI goes through our servers, then our AI provider (OpenAI): it needs a free account and has a daily limit.
A full 3D model, with AI
A well-prepared model avoids a lot of failed prints. The Nyzora studio uses AI to build a full 3D model from a photo or a sentence: 190 free credits at sign-up, with a quote before every charge.
Frequently asked questions
- Why is my resin print stuck to the FEP?
- Because the base didn't grip the plate hard enough, so the film won the tug of war on the lift. Raise bottom exposure by 5–10 s, keep 4–6 bottom layers, and check plate leveling and resin temperature (22–30 °C). A scratched or slack film needs replacing.
- How do I avoid the suction cup effect on a hollow print?
- A closed cavity pulls a vacuum on every lift. Add at least two drain holes of 3–5 mm, one near the plate and one on the far side, keep walls at 1.5–3 mm, and never point an open cavity at the film.
- Why is my print still tacky after curing?
- Most often it wasn't washed enough: liquid resin stays on the surface and never fully hardens. Two baths of 90 %+ isopropyl alcohol, the second one clean, a full dry, then 2–5 min of UV per side. Water-washable resin gets rinsed in clean water and dried before curing.
- Why do my resin prints crack a few days later?
- Three causes come up: too much UV, which makes resin brittle; resin trapped inside a closed hollow part; or a long soak in alcohol, which swells the surface and then crazes it. A few minutes of UV per side, drain holes, and 10 min of washing at most.
- Does it know my resin printer?
- It doesn't ask for the brand: causes and settings apply to common MSLA printers, whether you slice in Chitubox, Lychee or the maker's own software. Exact values depend on the resin, so start from its data sheet and adjust in small steps.
- What's free, and what do I pay for?
- The defect guide is free, with no account. The AI photo check is free with an account: 3 a day, 20 for subscribers.
- Is my photo uploaded?
- For the AI diagnosis, yes: the photo and any details you add go through our servers, with your account, and are analyzed by our AI provider (OpenAI). Nyzora does not keep them. The defect guide needs no photo and no account.